Chemical transformation of a substrate comprising wood, comprises two impregnation steps comprising: contacting the substrate comprising wood with a first liquid based treatment solution (at least 50 wt.%, preferably at least 80 wt.%) comprising a mixture containing 5-60 wt.% of glycerol and 40-95 wt.% of water; and contacting the substrate comprising wood with a second liquid based treatment solution (at least 50 wt.%, preferably at least 80 wt.%) comprising a mixture containing 5-90 wt.% of one or more dicarboxylic acids (I) and 10-95 wt.% of water. Chemical transformation of a substrate comprising wood, comprises impregnation steps comprising: contacting the substrate comprising wood with a first liquid based treatment solution (at least 50 wt.%, preferably at least 80 wt.%) comprising a mixture containing 5-60 wt.% of glycerol and 40-95 wt.% of water; and contacting the substrate comprising wood with a second liquid based treatment solution (at least 50 wt.%, preferably at least 80 wt.%) comprising a mixture containing 5-90 wt.% of one or more dicarboxylic acids of formula (HOOC-(CH 2) n-COOH) (I) and 10-95 wt.% of water. n : 6-10.
机译:包含木材的基材的化学转化包括两个浸渍步骤,该步骤包括:使包含木材的基材与第一液体基处理溶液(至少50 wt。%,优选至少80 wt。%)接触,该溶液包含5-60 wt%的混合物。 。%的甘油和40-95 wt。%的水;使包含木材的基材与第二液体基处理溶液(至少50 wt。%,优选至少80 wt。%)接触,该第二溶液包含含有5-90 wt。%的一种或多种二元羧酸(I)和10的混合物-95重量%的水。包含木材的基材的化学转化包括浸渍步骤,所述浸渍步骤包括:使包含木材的基材与第一液体基处理溶液(至少50 wt。%,优选至少80 wt。%)接触,该溶液包含5-60 wt。%的混合物。 %的甘油和40-95 wt。%的水;使包含木材的基材与第二液体基处理溶液(至少50 wt。%,优选至少80 wt。%)接触,该溶液包含含有5-90 wt。%的一种或多种式(HOOC- (CH 2)n-COOH)(I)和10-95 wt。%的水。 n:6-10。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号