Formulation for Producing a Writing Article, Process for Manufacturing a Writing Article and a Writing Article

机译:写作作品的制作方法,写作文章的制作过程以及写作文章

摘要

“FORMULATION FOR PRODUCING A WRITING ARTICLE, PROCESS FOR MANUFACTURING A WRITING ARTICLE AND A WRITING ARTICLE”, wherein the formulation of said writing article can optionally comprise the following components (with a variation of ±2.5%): ABS (Acrylonitrile-Butadiene-Styrene, 37-50%), SAN (Styrene-Acrylonitrile, 14%), Graphite (35-42%), Calcium Stearate (5-10%), Stearin (8%), Talc (5-23%), Mineral Oil (2-3%), Polyethylene (1%), Bentonite (5-15%), Calcium Carbonate (1%). Said article (1) is defined as a single-piece object (2), which has an integral tip (3) that is produced by sharpening; the body of said single-piece object (2) is configured according to a profile standard, and may include multiple sides (4) giving said single-piece object an hexagonal appearance, or even only one encircling side (5), which gives said single-piece object a cylindrical appearance. The manufacturing process consists of the following steps: (a) weighing the raw materials; (b) homogenizing the raw materials using mixing equipment, into which all of the raw materials are fed; (c) feeding the mixture obtained after processing the raw materials in the mixer into a piece of equipment called a pelletizing extruder; (d) feeding the granulated material obtained after processing the mixture in the pelletizing extruder into a second extruder; (e) producing a continuous graphite bar; (f) cutting the graphite bar into bar sections of adequate length according to the size of a pencil; (g) sharpening the graphite sections; and (h) printing, a step that defines obtaining the final product: a writing article (1), which can then be packaged.
机译:“用于生产书写制品的制剂,用于制造书写制品的过程和用于书写制品的制剂”,其中所述书写制品的制剂可任选地包含以下组分(变化为±2.5%):ABS(丙烯腈-丁二烯-苯乙烯) ,37-50%),SAN(苯乙烯-丙烯腈,14%),石墨(35-42%),硬脂酸钙(5-10%),硬脂酸(8%),滑石粉(5-23%),矿物油(2-3%),聚乙烯(1%),膨润土(5-15%),碳酸钙(1%)。所述物品( 1 )被定义为一件物品( 2 ),该物品具有一体式尖端( 3 ),该尖端是由锐化所述单一对象的主体( 2 )的主体根据轮廓标准配置,并且可以包括多个侧面( 4 ),使所述单一对象的外观呈六边形或什至只有一个环绕的侧面( 5 ),这使所述一体式物体具有圆柱形外观。制造过程包括以下步骤:(a)称量原材料; (b)使用混合设备将原料均质化,将所有原料加入其中; (c)将在混合器中对原料进行加工后获得的混合物供入称为造粒挤出机的设备中; (d)将在造粒挤出机中处理混合物后获得的粒状材料进料到第二挤出机中; (e)生产连续的石墨棒; (f)根据铅笔的大小将石墨棒切成足够长的棒部分; (g)锐化石墨部分; (h)印刷,这是定义获得最终产品的步骤:书写物品( 1 ),然后可以包装该物品。

著录项

  • 公开/公告号US2013330112A1

    专利类型

  • 公开/公告日2013-12-12

    原文格式PDF

  • 申请/专利权人 MAX LEE;

    申请/专利号US201213991084

  • 发明设计人 MAX LEE;

    申请日2012-06-19

  • 分类号B43K19/02;

  • 国家 US

  • 入库时间 2022-08-21 16:07:05