PROBLEM TO BE SOLVED: To provide a heat shrinkable film small in tensile elongation, excellent in low-temperature shrinkability and excellent even in appearance after shrinkage.;SOLUTION: The method for manufacturing a heat shrinkable polyethylene film comprises the steps of: (A) forming an inflation film by subjecting a polyethylene resin including a low density polyethylene as a principal component to inflation molding so as to become a blow ratio (a draw ratio) of 3.0-6.0 times in a longitudinal direction and a horizontal direction at a temperature equal to or more than the melting point of the low density polyethylene; and (B) further drawing the inflation film formed in the step (A) to 1.1-3.0 times in at least one direction at a temperature equal to or less than the melting point of the low density polyethylene.;COPYRIGHT: (C)2015,JPO&INPIT
机译:解决的问题:为了提供拉伸伸长率小,低温收缩性优异并且收缩后甚至外观优异的热收缩膜。解决方案:制造热收缩聚乙烯膜的方法包括以下步骤:(A)通过使包括低密度聚乙烯作为主要成分的聚乙烯树脂经受膨胀模制以在纵向和水平方向上在相等的温度下在纵向和横向上的吹塑比(拉伸比)为3.0-6.0倍来形成膨胀膜。达到或高于低密度聚乙烯的熔点; (B)在等于或小于低密度聚乙烯的熔点的温度下,在至少一个方向上进一步将步骤(A)中形成的膨胀膜拉伸至1.1-3.0倍。;版权所有:(C)2015 ,JPO&INPIT

著录项

  • 公开/公告号JP2015063650A

    专利类型

  • 公开/公告日2015-04-09

    原文格式PDF

  • 申请/专利权人 SEKISUI FILM KK;

    申请/专利号JP20140018606

  • 发明设计人 KOBAYASHI TAKAAKI;KITAHARA EIJI;

    申请日2014-02-03

  • 分类号C08J5/18;B29C55/28;B29C61/06;B65D65/02;B29K23;B29K105/02;B29L7;

  • 国家 JP

  • 入库时间 2022-08-21 15:32:51

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号