The present invention relates to a method for producing organic calcium hydroxide and organic nano calcium carbonate using shells, which are usually disposed. The method includes the steps of: washing the shells; sintering the washed shells at 1,200°C for 30-60 minutes after increasing the temperature up to 1,200°C at a speed of 10°C per minute; cooling the shells after the temperature of a sintering furnace is cooled down to be 400-600°C after the sintering step and then taking out of the sintered shells; quenching 100 g of the sintered shells with 300-600 g of water and agitating the sintered shells at a rational speed of 200-400 per minute for 30 minutes; filtrating the shells to separate the shells into powder slurry and a filtrate after agitation; obtaining organic calcium hydroxide by injecting carbon dioxide into the filtrate and maintaining the reaction temperature of the inside of a reactor to be 400-600°C and maintaining the rotational speed per minute to be 100-300; and obtaining dried organic calcium carbonate powder by drying the organic nano calcium carbonate at 100±10°C.;COPYRIGHT KIPO 2015
机译:本发明涉及使用通常配置的壳来制造有机氢氧化钙和有机纳米碳酸钙的方法。该方法包括以下步骤:洗涤壳;在以每分钟10℃的速度将温度升至1200℃之后,将洗涤后的壳在1200℃下烧结30-60分钟;在烧结步骤后将烧结炉的温度冷却至400-600℃后冷却壳,然后从烧结的壳中取出;用300-600g水淬灭100g烧结的壳,并以200-400 / min的合理速度搅拌烧结的壳30分钟;过滤壳,搅拌后将壳分离成粉浆和滤液;通过向滤液中注入二氧化碳并保持反应器内部的反应温度为400-600℃并且保持每分钟的旋转速度为100-300,获得有机氢氧化钙。并通过将有机纳米碳酸钙在100 + 10°C下干燥得到有机碳酸钙干粉。COPYRIGHTKIPO 2015

著录项

  • 公开/公告号KR20150084701A

    专利类型

  • 公开/公告日2015-07-22

    原文格式PDF

  • 申请/专利权人 KUMHO CO. LTD.;

    申请/专利号KR20150066401

  • 申请日2015-05-13

  • 分类号C01F11/18;

  • 国家 KR

  • 入库时间 2022-08-21 14:59:33

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号