摘要

FIELD: chemistry.SUBSTANCE: invention relates to production of a precursor based on titanium dioxide for catalytically active coating on an inert carrier containing nano-sized metal particles of palladium. Colloidal solution of a siloxane-acrylate emulsion, while stirring, is mixed with a solution of tetrachloropalladic acid HPdCland under constant stirring are heated at a temperature of 75-80°C. Resulting solution is cooled followed by reduction of palladium from ionic form to metal in form of nanoparticles by adding a reducing solution of titanium(III) chloride in hydrochloric acid, followed by stirring resulting colloidal solution for a time sufficient for complete hydrolysis and polycondensation to form hydrated titanium dioxide TiO·nHO.EFFECT: obtaining thermally stable oxide coating containing palladium nanoparticles, using said precursor.5 cl, 1 tbl, 1 ex
机译:技术领域本发明涉及基于二氧化钛的前体的生产,该前体用于在包含纳米级钯金属颗粒的惰性载体上催化活性涂层。在搅拌下,将硅氧烷-丙烯酸酯乳液的胶体溶液与四氯钯酸HPdCland的溶液在恒定搅拌下混合,并在75-80℃的温度下加热。冷却所得溶液,然后通过加入氯化钛(III)在盐酸中的还原溶液,将钯从离子形式还原为纳米颗粒形式的金属,然后搅拌所得的胶体溶液足够的时间以完全水解和缩聚形成。水合二氧化钛TiO·nHO。效果:使用所述前体获得含有钯纳米粒子的热稳定氧化物涂层。5 cl,1 tbl,1 ex

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号