摘要

PROBLEM TO BE SOLVED: To provide a method capable of producing high-purity perrhenic acid from rhenium sulfide obtained by treating an acidic solution containing rhenium using a dry process.SOLUTION: There is provided a method for producing a perrhenic acid aqueous solution which comprises: a step of passing an acidic solution containing rhenium through an anion exchange resin to adsorb rhenium on the anion exchange resin; a step of passing an eluent through the anion exchange resin on which rhenium is adsorbed to elute rhenium from the anion exchange resin; a step of sulfurizing the rhenium contained in a solution after elution to obtain rhenium sulfide; a step of subjecting the rhenium sulfide to first burning in the presence of an oxygen-containing gas to generate rhenium oxide and a sulfur oxide and gasifying and discharging the sulfur oxide to obtain rhenium oxide as a burning residue; a step of subjecting the burning residue to second burning in the presence of an oxygen-containing gas to collect the gasified rhenium oxide; a step of cooling and solidifying the gasified rhenium oxide; a step of obtaining a perrhenic acid aqueous solution by dissolving the gasified rhenium oxide in water while cooling with water; and a step of obtaining the perrhenic acid aqueous solution by dissolving the solidified rhenium oxide in water, or heating and gasifying the solidified rhenium oxide and followed by dissolving in water, when the rhenium oxide is solidified.
机译:解决的问题:提供一种能够通过使用干法处理含containing的酸性溶液而获得的硫化rh生产高纯度高r酸的方法。解决方案:提供了一种生产高acid酸水溶液的方法,该方法包括:使含有rh的酸性溶液通过阴离子交换树脂以使rh吸附在阴离子交换树脂上的步骤。使洗脱液通过吸附有rh的阴离子交换树脂以从该阴离子交换树脂上洗脱ium的步骤;洗脱后将溶液中所含的sulfur硫化,得到硫化rh的步骤。硫化the首先在含氧气体存在下燃烧,生成氧化rh和氧化硫,然后将其氧化气化并排出,得到氧化burning作为燃烧残渣的步骤;在含氧气体的存在下对燃烧残渣进行第二次燃烧以收集气化的氧化ium的步骤;冷却并固化气化的氧化oxide的步骤;通过将气化的氧化oxide溶解在水中并用水冷却而获得高r酸水溶液的步骤;通过将固化的氧化oxide溶解在水中,或者将固化的氧化en加热并气化,然后将其溶解在水中而获得高r酸水溶液的步骤。

著录项

  • 公开/公告号JP2016014167A

    专利类型

  • 公开/公告日2016-01-28

    原文格式PDF

  • 申请/专利权人 PAN PACIFIC COPPER CO LTD;

    申请/专利号JP20140136094

  • 发明设计人 SUMIDA IKUNOBU;KONO TAKEHITO;

    申请日2014-07-01

  • 分类号C22B61;C22B3/42;C22B1/02;C01G47;

  • 国家 JP

  • 入库时间 2022-08-21 14:45:23

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号