PROBLEM TO BE SOLVED: To provide a lithium cobaltate orientated sintered plate which is hard to cause a trouble in a battery performance even if a LiPON based solid electrolyte layer is formed on its surface by sputtering.SOLUTION: A method for manufacturing a lithium cobaltate orientated sintered plate comprises (a)a step for preparing a green sheet including CoOparticles; (b)a step for sintering the green sheet into a CoOoriented sintered plate; and (c)a step for sintering the CoOoriented sintered plate in coexistence of a lithium source to introduce lithium thereinto, thereby forming the lithium cobaltate orientated sintered plate primarily including LiCoO. The method further comprises: (d1)a step for covering a surface of the CoOoriented sintered plate with a liquid solution or slurry of a compound including at least one additive element of Ti, Al and/or Zr prior to the step (c); or (d2)a step for coating the surface of the lithium cobaltate oriented sintered material with the liquid solution or slurry and then, sintering the lithium cobaltate oriented sintered material coated with the liquid solution or slurry after the step (c).SELECTED DRAWING: None
机译:解决的问题:提供即使在通过溅射在表面上形成了LiPON系固体电解质层的情况下,也不会对电池性能造成不良影响的钴酸锂取向烧结板。解决方案:一种锂钴酸锂取向烧结板的制造方法。烧结板包括(a)制备包含CoO颗粒的生片的步骤; (b)将生片烧结成CoO取向的烧结板的步骤; (c)在锂源共存的状态下烧结CoO取向烧结板而向其中导入锂的工序,从而形成以LiCoO为主成分的钴酸锂取向烧结板。该方法进一步包括:(d1)在步骤(c)之前,用包含至少一种Ti,Al和/或Zr的添加元素的化合物的液体溶液或浆料覆盖CoO取向的烧结板的表面的步骤;或(d2)用液体溶液或浆料涂覆钴酸锂取向的烧结材料的表面,然后在步骤(c)之后烧结涂覆有液体溶液或浆料的钴酸锂取向的烧结材料的步骤。没有

著录项

  • 公开/公告号JP2016072241A

    专利类型

  • 公开/公告日2016-05-09

    原文格式PDF

  • 申请/专利权人 NGK INSULATORS LTD;

    申请/专利号JP20150181802

  • 申请日2015-09-15

  • 分类号H01M4/1391;H01M10/0562;H01M10/0585;H01M4/131;H01M4/525;H01M4/62;C01G51;C04B35;

  • 国家 JP

  • 入库时间 2022-08-21 14:42:30

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号