首页> 外国专利> Process for the preparation of monolithic structures catalyst used in the synthesis of the dialkyl oxalate with CO gas phase coupling, and a manufacturing method of the dialkyl oxalate

Process for the preparation of monolithic structures catalyst used in the synthesis of the dialkyl oxalate with CO gas phase coupling, and a manufacturing method of the dialkyl oxalate

机译:草酸二烷基酯与CO气相偶联合成中使用的整体结构催化剂的制备方法及草酸二烷基酯的制备方法

摘要

[Problems] The present invention provides for the use and process for its preparation and a monolithic catalyst structure used for the synthesis of oxalate by CO gas phase coupling. The carrier and the skeleton metal honeycomb or ceramic honeycomb, and a wash coat layer of metal oxide, and an active ingredient a noble metal Pt, Pd, Ir, and Rh, monolithic structures catalysts of the present invention comprises, Fe, Co , I and aid Ni. The wash coat layer, accounted for 5-50% of the honeycomb carrier, accounting for 0.1 to 5 wt% of the washcoat layer, the auxiliaries of the catalyst active component of the catalyst, 0.3 washcoat layer accounts for 10 wt%, the atomic ratio of active ingredient to aid is 0.1 to 3. The synthesis reaction of oxalic acid salt, and a carrier gas N 2, 2 N: 5~60:: volume ratio = 20 to 80 of the alkyl nitrite: CO 10~40, dwell time is 0.5 to 10 seconds, is performed in a fixed bed reactor.
机译:[问题]本发明提供了其制备的用途和方法以及用于通过CO气相偶联合成草酸酯的整体催化剂结构。本发明的整体结构催化剂的载体和骨架金属蜂窝或陶瓷蜂窝,金属氧化物的洗涂层和活性成分贵金属Pt,Pd,Ir和Rh包括单质结构催化剂。并帮助倪洗涂层占蜂窝载体的5-50%,占洗涂层的0.1-5wt%,催化剂的催化剂活性成分的助剂,0.3洗涂层占原子的10wt%。活性成分与助剂的比例为0.1:3。草酸盐与载气 N 2、2 N:5〜60 :: 的合成反应体积比为20至80亚硝酸盐:CO 10〜40,停留时间为0.5至10秒,在固定床反应器中进行。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号