Method for the assessment of the effectiveness of the process of high-chromium cast iron modification

机译:评估高铬铸铁改性过程有效性的方法

摘要

evaluation of effectiveness wysokochromowego procedure modification iron containing 8 - 25% w / w cr is characterized by the fact that the molten metal before and after surgery modification urinating into shape, having at least two recess of circular or square and the dia dnicy or length of side of 5 to 30 mm.with the obtained rods performs samples for research metalograficznych which undergo digestion, and then under the microscope counts the quantity of grains ru00f3wnoosiowych. the effect of the modification is satisfactory if the number of grains ru00f3wnoosiowych in samples after surgery the modification is at least about 50% greater than the number of grains ru00f3wnoosiowych obtained in samples without treatment modifications.
机译:ws / w cr含量为8-25%的Wysokochromowego程序改性铁的有效性评估,其特征在于,手术改性前后的熔融金属呈小便状,具有至少两个圆形或正方形的凹口,直径或长度用获得的棒对5至30mm的边进行取样,以进行研究金属样品的消化,然后在显微镜下计数r u00f3wnoosiowych的颗粒数量。如果修饰后的手术后样品中的晶粒数比未经处理修饰的样品中获得的晶粒数大至少约50%,则修饰的效果令人满意。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号