The invention relates to a method for producing a three-dimensionally shaped steel component from a steel sheet which has a metal coating and which is heated and subsequently shaped into the steel component by means of a hot-forming process. The steel sheet used has an Fe-Al-based alloy as a metal coating. In order to protect the steel sheet or the steel component from scaling, an Fe-Al-based alloy is applied directly onto the steel sheet by means of a galvanic coating process and/or a physical vapor phase deposition, wherein the coating produced in this manner contains 30 - 60 wt.% Fe, a group of Al, and optionally 0.1 - 10 wt.% Mg and/or 0.1 - 5 wt.% Ti and/or 0.1 - 10 wt.% Si and/or 0.1 - 10 wt.% Li and/or 0.1 - 10 wt.% Ca, and the alloy has an Fe-Al phase which is stable up to over 900 °C prior to the heating process to be carried out for the hot-forming process. The invention further relates to a correspondingly coated steel sheet for producing one or more steel components produced by means of a hot-forming process.
机译:本发明涉及一种由具有金属涂层的钢板生产三维形状的钢构件的方法,该钢板被加热并随后通过热成型工艺成形为钢构件。所使用的钢板具有Fe-Al基合金作为金属涂层。为了保护钢板或钢构件免于结垢,通过电镀方法和/或物理气相沉积将Fe-Al-基合金直接施加到钢板上,其中以这种方式产生的涂层该方式包含30-60重量%的Fe,一组铝,和任选地0.1-10重量%的Mg和/或0.1-5重量%的Ti和/或0.1-10重量%的Si和/或0.1-10重量%的Li和/或0.1-10重量%的Ca,并且该合金具有Fe-Al相,该Fe-Al相在用于热成型过程的加热过程之前在高达900℃以上的温度下都稳定。本发明还涉及一种用于生产一种或多种通过热成型方法生产的钢构件的相应涂覆的钢板。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号