Task A zinc recovery method from an electric furnace steelmaking dust capable of recovering high purity zinc metal in a relatively short time and a zinc recovery apparatus from an electric furnace steelmaking dust are provided. [Solution] Ca mixed heating means 11 is used to mix the electric furnace-making dust and the calcium compound and heat-treated in a non-reducing atmosphere at 960 ° C to 1100 ° C for 1 to 3 hours to obtain ZnO and 2CaO · Fe 2 O 3 . The iron powder mixing means 12 mixes the iron powder with the ZnO and 2CaO 占2 2 O 3 and mixes them. The green compact 1 is disposed inside the decompression vessel 21 with the reducing and volatilizing means 13 and the inside of the decompression vessel 21 is decompressed and heated to generate the zinc vapor 2, The steam (2) is cooled and solidified to obtain a solid zinc metal piece (3). The zinc metal piece (3) is dissolved in a multi-component chloride-based flux based on NaCl-KCl by the zinc acquisition means (14) and then cooled to obtain massive zinc.
机译:<任务>提供一种能够在相对短的时间内回收高纯度锌金属的从电炉炼钢粉尘中回收锌的方法以及从电炉炼钢粉尘中回收锌的设备。 [解决方案]使用Ca混合加热装置11将电炉中产生的粉尘和钙化合物混合,并在非还原性气氛中于960℃至1100℃下进行1至3小时的热处理,从而获得ZnO和2CaO。 ·Fe 2 O 3 。铁粉混合装置12将铁粉与ZnO和2CaO占 2 2 O 3 混合并混合。生坯1通过减压挥发装置13配置在减压容器21的内部,对减压容器21的内部进行减压加热而生成锌蒸气2,将蒸气(2)冷却固化而得到固体。锌金属片(3)。通过锌获取装置(14)将锌金属片(3)溶解在基于NaCl-KCl的多组分氯化物基焊剂中,然后冷却以获得块状锌。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号