Hydrometallurgical recovery of zinc from electric arc furnace dust was investigated on a laboratory scale, using aqueous sodium hydroxide solution as a leaching agent. Special attention was paid to the effect of NaOH concentration, temperature and liquid/solid phase ratio on the zinc leachability. It was found that all tested factors increased the leachability, with the maximum efficiency of 88% obtained in a 6 M NaOH solution at a temperature of 80 °C and the liquid/solid phase ratio of 40. The test results confirmed the high selectivity of the zinc leaching agent. In spite of this, complete recovery of zinc from steelmaking dust has proved to be very difficult due to the occurrence of this element in the form of stable and sparingly soluble ZnFe 2 O 4 ferrite. Purification of the solution by cementation and electrolysis gave zinc of purity 99.88% in powder form.
机译:使用氢氧化钠水溶液作为浸出剂,在实验室规模上研究了从电弧炉粉尘中湿法冶金回收锌。特别注意NaOH浓度,温度和液/固比对锌浸出率的影响。发现所有测试因素均提高了浸出率,在温度为80°C,液相/固相比为40的6 M NaOH溶液中,其最高效率为88%。测试结果证实了高选择性。锌浸出剂。尽管如此,由于以稳定且微溶的ZnFe 2 O 4铁氧体形式存在该元素,已证明很难从炼钢粉尘中完全回收锌。通过胶凝和电解对溶液进行纯化,得到呈粉末形式的纯度为99.88%的锌。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号