SYNTHESIS OF LIFEPO4 UNDER HYDROTHERMAL CONDITIONS

机译:水热条件下合成LIFEPO4

摘要

The present invention relates to a process for the preparation of a compound of formula (I) (A) at least one lithium containing compound, at least one iron containing compound having an oxidation number of iron of +3, and at least one M 1 containing compound, if present, and / or at least one M 2 containing compound, and / Providing a mixture comprising at least one M 3 containing compound and at least one reducing agent oxidized to at least one compound comprising at least one phosphorus atom of oxidation number +5, and (B) reducing the Fe to an oxidation number of +2 by heating the mixture obtained in step (A) at a temperature of 100 to 500 DEG C and a magnetic pressure to obtain a compound of formula (I) RTI ID = 0.0 : / RTI & Li ab M 1b Fe 1-c M 2c P de M 3e O x (I) Wherein, The oxidation number of Fe is +2, M 1 : Na, K, Rb and / or Cs, M 2 : Mn, Mg, Al, Ca, Ti, Co, Ni, Cr, V, M 3 : Si, S, F, a: 0.8 to 1.9, b: 0 to 0.3, c: 0 to 0.9, d: 0.8 to 1.9, e: 0 to 0.5, x: 1.0 to 8, depending on the amount of Li, M 1 , M 2 , P and M 3 and the oxidation number.
机译:本发明涉及一种制备式(I)(A)化合物的方法,该方法包括至少一种含锂化合物,至少一种铁的氧化数为+3的含铁化合物以及至少一种M <如果存在,则含有Sup> 1 的化合物,和/或至少一种含有M 2 的化合物,和/或提供包含至少一种含有M 3 的化合物的混合物化合物和至少一种还原剂被氧化成至少一种包含至少一个氧化数为+5的磷原子的化合物,以及(B)通过将在步骤(A)中获得的混合物加热至70℃,将Fe还原为+2。在100至500℃的温度和磁压下获得式(I)的化合物: Sub M 1 b Fe 1-c M 2 c P de M 3 e O x (I)其中,Fe的氧化数为+ 2,M 1 :Na,K,Rb一个d /或Cs,M 2 :Mn,Mg,Al,Ca,Ti,Co,Ni,Cr,V,M 3 :Si,S,F,a :0.8到1.9,b:0到0.3,c:0到0.9,d:0.8到1.9,e:0到0.5,x:1.0到8,取决于Li的量,M 1 ,M 2 ,P和M 3 以及氧化数。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号