The present invention relates to an aqueous solution containing at least a nickel salt and a neutralizing agent which are supplied continuously to a reaction vessel with stirring and not containing a complex ion forming agent for forming a complex ion with a metal element in the reaction aqueous solution, The crystallization reaction is controlled so that the volume average particle diameter becomes 0.2 to 0.6 with respect to the secondary particles finally obtained, to obtain a nickel complex hydroxide slurry. Thereafter, while keeping the state that the complex ionizing agent is not contained, only the liquid component of the slurry is continuously removed while maintaining the capacity of the slurry obtained in the primary crystallization step, By controlling the pH value at 90 占 폚 and the liquid temperature at 25 占 폚 in the range of 10.0 to 11.0 and continuing the crystallization reaction until the secondary particles have a volume average particle diameter of 8.0 to 50.0 占 퐉, And a method for producing the same.
机译:本发明涉及至少包含镍盐和中和剂的水溶液,所述水溶液在搅拌下连续地供应至反应容器,并且不包含用于在反应水溶液中与金属元素形成复合离子的复合离子形成剂。通过控制结晶反应,使相对于最终得到的二次粒子的体积平均粒径为0.2〜0.6,得到镍复合氢氧化物浆料。此后,在保持不包含络合电离剂的状态的同时,通过将pH值控制在90占폚的范围内并保持初始结晶步骤中获得的浆料的容量,而仅连续地除去浆料的液体成分。 25℃下的液相温度为10.0〜11.0的范围内,使结晶反应继续进行,直到二次粒子的体积平均粒径为8.0〜50.0℃下为止。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号