首页> 外国专利> MAGNETIC RUBBER COMPOSITION, MAGNETIC RUBBER MOLDED ARTICLE, MAGNETIC ENCODER AND MANUFACTURING METHOD THEREFOR

MAGNETIC RUBBER COMPOSITION, MAGNETIC RUBBER MOLDED ARTICLE, MAGNETIC ENCODER AND MANUFACTURING METHOD THEREFOR

机译:磁性橡胶组合物,磁性橡胶模制件,磁性编码器及其制造方法

摘要

PROBLEM TO BE SOLVED: To provide a magnetic rubber molded article having both of extremely excellent magnetic property and good mechanical properties by vulcanizing a magnetic rubber composition excellent in flowability while containing a magnetic powder at extremely high concentration.SOLUTION: There is provided a magnetic rubber composition containing a hydrogenated nitrile rubber (A), a magnetic ferrite powder (B), a vulcanizer (C) and stearic acid (D) with Mooney viscosity (ML, 100°C) of the hydrogenated nitrile rubber (A) of 45 to 80, containing the magnetic ferrite powder (B) of 1250 to 1600 pts.mass, the vulcanizer (C) of 0.1 to 4 pts.mass and the stearic acid (D) of 2.5 to 8 pts.mass based on 100 pts.mass of the hydrogenated nitrile rubber and having percentage content of the magnetic ferrite powder (B) to mass of whole magnetic rubber composition of 91 to 93 mass%.SELECTED DRAWING: None
机译:要解决的问题:通过硫化流动性优异的磁性橡胶组合物同时含有极高浓度的磁性粉末,从而提供兼具极优异的磁性和机械性能的磁性橡胶成型品。组合物,其包含氢化丁腈橡胶(A)的门尼粘度(ML,100℃)为45〜45℃的氢化丁腈橡胶(A),铁氧体磁粉(B),硫化剂(C)和硬脂酸(D)。 80,包含质量为1250至1600 pts的磁性铁氧体粉末(B),质量为0.1至4 pts的硫化剂(C)和基于100 pts.mass的硬脂酸(D)的质量为2.5至8 pts。氢化丁腈橡胶的含量,并且磁性铁氧体粉末(B)的含量相对于整个磁性橡胶组合物的质量为91到93质量%。

著录项

  • 公开/公告号JP2017095539A

    专利类型

  • 公开/公告日2017-06-01

    原文格式PDF

  • 申请/专利权人 UCHIYAMA MANUFACTURING CORP;

    申请/专利号JP20150226082

  • 发明设计人 SAKATE KAZUSHI;KASAMOTO TADASHI;KAWAI RYO;

    申请日2015-11-18

  • 分类号C08L15;C08K3/22;C08K5/09;C08J3/20;H01F7/02;H01F41/02;

  • 国家 JP

  • 入库时间 2022-08-21 13:59:41

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号