Method for producing lithium lanthanum titanium oxide sintered body, method for producing solid electrolyte containing said oxide, and method for producing lithium-air battery and all-solid lithium battery comprising said solid electrolyte

机译:锂镧钛氧化物烧结体的制造方法,含有该氧化物的固体电解质的制造方法,以及含有该固体电解质的锂空气电池和全固体锂电池的制造方法

摘要

A lithium-lanthanum-titanium oxide sintered material has a lithium ion conductivity 3.0 x 10 -4 Scm -1 or more at a measuring temperature of 27 °C, the material is described by one of general formulas (1-a)La x Li 2-3x TiO 3 -aSrTiO 3 , (1-a)La x Li 2-3x TiO 3 -aLa 0.5 K 0.5 TiO 3 , La x Li 2-3x Ti 1-a M a O 3-a , Sr x-1.5a La a Li 1.5-2x Ti 0.5 Ta 0.5 O 3 (0.55 ‰¤ x ‰¤ 0.59, 0 ‰¤ a ‰¤ 0.2, M = at least one of Fe or Ga), amount of Al contained is 0.35 mass% or less as Al 2 O 3 , amount of Si contained is 0.1 mass% or less as SiO 2 , and average particle diameter is 18 µm or more.
机译:锂-镧-钛氧化物烧结材料在27℃的测量温度下具有3.0×10 -4 Scm -1或更高的锂离子电导率,该材料由通式(1-a)La x Li描述。 2-3x TiO 3 -aSrTiO 3,(1-a)La x Li 2-3x TiO 3 -aLa 0.5 K 0.5 TiO 3,La x Li 2-3x Ti 1-a M a O 3-a,Sr x- 1.5a La a Li 1.5-2x Ti 0.5 Ta 0.5 O 3(0.55‰x‰0.59,0‰a‰¤0.2,M = Fe或Ga中至少一种),Al的含量为0.35质量% Al 2 O 3为0以下,Si的含有量为SiO 2为0.1质量%以下,平均粒径为18μm以上。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号