首页> 外国专利> Stress luminescent material, method for producing stress luminescent material, stress luminescent coating composition, resin composition, and stress luminescent material

Stress luminescent material, method for producing stress luminescent material, stress luminescent coating composition, resin composition, and stress luminescent material

机译:应力发光材料,应力发光材料的制造方法,应力发光涂料组合物,树脂组合物和应力发光材料

摘要

A stress-stimulated luminescent material obtained by mixing a phosphate compound and europium activated strontium aluminate particles to prepare a slurry, a pulverizing step of pulverizing the slurry to obtain a pulverized slurry, and a drying step of drying the pulverized slurry The content A of the strontium element in the obtained stress-stimulated luminescent material and the content B of the strontium element after the stress-stimulated luminescent material was held for 168 hours in an atmosphere at a temperature of 85 ° C. and a relative humidity of 85%. A stress luminescent material characterized in that the rate of change calculated by (AB) / A × 100 is 10% or less.
机译:通过将磷酸盐化合物和euro活化铝酸锶锶颗粒混合以制备浆料而获得的应力刺激的发光材料,将浆料粉碎以获得粉碎浆料的粉碎步骤,以及将粉碎浆料干燥的干燥步骤。将获得的应力刺激的发光材料中的锶元素和应力刺激的发光材料之后的锶元素的含量B在温度为85℃,相对湿度为85%的气氛中保持168小时。一种应力发光材料,其特征在于,由(AB)/ A×100计算出的变化率为10%或更小。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号