首页> 外国专利> methods for controllably producing a hematite-containing fischer-tropsch catalyst and for producing hematite-containing fischer-tropsch hydrocarbon product, and

methods for controllably producing a hematite-containing fischer-tropsch catalyst and for producing hematite-containing fischer-tropsch hydrocarbon product, and

机译:可控制地生产含赤铁矿的费-托催化剂的方法和生产含赤铁矿的费-托烃产品的方法,和

摘要

1/1 Summary “Methods to Controllably Produce a Hematite-containing Fischer-Tropsch Catalyst and to Produce Fischer-Tropsch Hydrocarbon Product, Product, and, Hematite-containing Fischer-Tropsch Catalyst” controllably a hematite-containing fischer-tropsch catalyst by combining an iron nitrate solution with a precipitating agent solution at a precipitating temperature. and over a precipitation time to form a precipitate comprising iron phases; maintaining the precipitate at a retention temperature for a retention time to provide a hematite containing precipitate; and washing the hematite containing precipitate by contact with a wash solution and filtering to provide a washed hematite containing catalyst. The method may further comprise promoting the hematite-containing catalyst washed with a chemical promoter; spray drying the promoted hematite-containing catalyst; and calcining the spray dried hematite-containing catalyst to provide a calcined hematite-containing fischer-tropsch catalyst.
机译:1/1总结“通过可控地结合使用在沉淀温度下将硝酸铁溶液与沉淀剂溶液混合。在沉淀时间内形成包含铁相的沉淀;将沉淀物在保持温度下保持一段时间,以提供含赤铁矿的沉淀物;通过与洗涤溶液接触并过滤,洗涤含赤铁矿沉淀物,以提供洗涤后的含赤铁矿催化剂。该方法可以进一步包括促进用化学促进剂洗涤的含赤铁矿催化剂;和喷雾干燥促进的含赤铁矿催化剂;煅烧该喷雾干燥的含赤铁矿的催化剂,以提供煅烧的含赤铁矿的费歇尔-托普施催化剂。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号