首页> 外国专利> METHOD OF TREATMENT OF FLYING ASH AND USED FOR THIS ROTARY MILL

METHOD OF TREATMENT OF FLYING ASH AND USED FOR THIS ROTARY MILL

机译:粉煤灰的处理方法及用于该旋磨机的方法

摘要

1. A method of processing fly ash, as a result of which it can be used as a substitute for Portland cement in concrete production, comprising the step of: grinding fly ash having at least two components in a rotary mill having working bodies of various sizes and shapes, thus that the mill increases the total surface of these two different components of fly ash to provide activated fly ash. 2. The method according to claim 1, wherein the first component of the fly ash includes non-spherical particles, and the second component of the fly ash includes spherical components. The method according to claim 2, wherein the working bodies of various sizes and shapes reduce the size of the nonspherical components of the fly ash, while grinding the surface with the spherical fly ash component, thereby increasing the total surface of both components. A method according to claim 3, wherein the total total surface of the fly ash that has undergone grinding is increased by at least 30%, thereby giving the fly ash more reactivity. The method according to claim 1, wherein the rotary mill grinds calcium together with the components of fly ash. The method of claim 5, wherein the calcium comprises at least one of the following: quicklime, slaked lime, calcium carbonate, calcium formate, calcium nitrate or a related calcium compound. The method of claim 5, wherein the rotary mill output includes calcium milled together with fly ash to form calcium coated fly ash particles. The method of claim 7, wherein the calcium coated fly ash particles are ground together with the fly ash in a subsequent step.
机译:1。一种处理粉煤灰的方法,其结果可以用作混凝土生产中的硅酸盐水泥的替代品,其包括以下步骤:在具有各种工作体的旋转磨机中研磨具有至少两种组分的粉煤灰。尺寸和形状,从而使磨粉机增加了粉煤灰这两种不同成分的总表面积,以提供活性粉煤灰。 2.根据权利要求1所述的方法,其中,所述飞灰的第一组分包括非球形颗粒,并且所述飞灰的第二组分包括球形组分。 3.根据权利要求2所述的方法,其中,各种尺寸和形状的工作体在用球形飞灰组分研磨表面的同时减小了飞灰的非球形组分的尺寸,从而增加了两种组分的总表面积。 4.根据权利要求3所述的方法,其特征在于,经过磨削的粉煤灰的总表面增加至少30%,从而使粉煤灰具有更高的反应性。 2.根据权利要求1所述的方法,其中,所述旋转磨机将钙与飞灰的成分一起研磨。 6.根据权利要求5所述的方法,其中所述钙包括以下至少一种:生石灰,熟石灰,碳酸钙,甲酸钙,硝酸钙或相关的钙化合物。 6.根据权利要求5所述的方法,其中,所述旋转磨机的输出包括与粉煤灰一起研磨的钙,以形成涂覆有钙的粉煤灰颗粒。 8.根据权利要求7所述的方法,其中在随后的步骤中将所述钙涂覆的飞灰颗粒与所述飞灰一起研磨。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号