The invention relates to a method for the production of an elastic deformation body from Al2O3 ceramics, utilizing a highly pure alumina having a maximum of 2000 ppm of MgO1, a maximum of 200 ppm of inorganic contaminants, a specific surface of at least 10 m2/g, a mean grain size of a maximum of 0.3 µm, wherein a homogeneous mixture is created using the alumina and additives by means of aqueous processing, from which a spray granulate that can be compressed is created, which is formed into a homogeneous green body by means of a uniaxial compressing method, the green body being subjected to a sintering process, wherein the resulting elastic deformation body has a bending rupture stress sc, the distribution F (sc ) of which is given by the Weibull parameters s0 = 800 MPa and m = 24, and has a mean grain size of the sintered material of less than 2 µm, and wherein the sintered material of the deformation body has a density of less than 3.98 g/m2.
机译:本发明涉及一种由Al 2 O 3陶瓷生产弹性变形体的方法,该方法利用具有最高2000ppm的MgO 1,最高200ppm的无机污染物,比表面积至少为10m 2 /的高纯氧化铝。 g,最大晶粒度最大为0.3 µm,其中使用氧化铝和添加剂通过水处理形成均质混合物,由此形成可压缩的喷雾颗粒,形成均匀的生坯通过单轴压缩方法,对生坯进行烧结处理,其中所得的弹性变形体具有弯曲断裂应力sc,其分布F(sc)由威布尔参数s0 = 800 MPa给出,并且m = 24,并且烧结材料的平均晶粒尺寸小于2μm,并且其中变形体的烧结材料的密度小于3.98g / m 2。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号