PROBLEM TO BE SOLVED: To provide an early-strength admixture which secures a pot life necessary for a work in any one of ordinary temperature and high temperature range ready for curing with steam, and then can achieve early-strength development of approximately 7.5 N/mm2 or more in an early period of 3-4 hours.;SOLUTION: An early-strength admixture for secondary product contains alumina cement, anhydrous gypsum, slaked lime, and a retarder, where a content ratio of the alumina cement is 47 to 57 mass%, a content ratio of the anhydrous gypsum is 27 to 40 mass%, a content ratio of the slaked lime is 6 to 14 mass%, a content ratio of the retarder is 1 to 6 mass%, and a ratio of the alumina cement to the anhydrous gypsum is 56:44 to 64:36 in a mass ratio of "alumina cement:anhydrous gypsum".;SELECTED DRAWING: None;COPYRIGHT: (C)2018,JPO&INPIT
机译:解决的问题:提供一种早期强度的混合物,该混合物可确保在常温和高温范围内的任何工作下都可以用蒸汽固化的适用期,并且可以实现约7.5 N / N的早期强度发展。 mm 2 或更高,在3-4小时内即可解决;解决方案:用于次要产品的早强混合料包含氧化铝水泥,无水石膏,熟石灰和缓凝剂,其含量比氧化铝水泥的含量为47〜57质量%,无水石膏的含量为27〜40质量%,熟石灰的含量为6〜14质量%,缓凝剂的含量为1〜6质量。 %,并且以“氧化铝水泥:无水石膏”的质量比,氧化铝水泥与无水石膏的比率为56:44至64:36 。;选定的图纸:无;版权:(C)2018,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号