PROBLEM TO BE SOLVED: To provide a method for reducing an amount of lithium remaining in positive electrode active material particles in a simple and efficient manner while suppressing the rise in the production cost.SOLUTION: A method for reducing an amount of lithium remaining in positive electrode active material particles made of a lithium composite oxide comprises at least the step of setting a baking temperature at a temperature of 850°C or higher, and keeping the set baking temperature and an ambient atmosphere for a given time and then, switching an atmosphere while the set baking temperature is lowered, from the ambient atmosphere to a low-carbon dioxide gas atmosphere of which the carbon dioxide concentration is no more than 1/60 of a carbon dioxide concentration of the ambient atmosphere, and baking a mixture of a precursor compound including Ni, Co and Mn, and a lithium compound, thereby preparing a lithium composite oxide.SELECTED DRAWING: None
机译:解决的问题:提供一种以简单有效的方式减少正极活性物质颗粒中锂残留量的方法,同时抑制生产成本的上升。解决方案:提供一种减少正极活性物质锂残留量的方法。由锂复合氧化物制成的电极活性材料颗粒至少包括以下步骤:将烘烤温度设定为850℃或更高的温度,并将设定的烘烤温度和环境气氛保持给定时间,然后切换气氛在降低设定的烘烤温度的同时,从周围大气到二氧化碳浓度为周围大气的二氧化碳浓度的1/60以下的低二氧化碳气体气氛,进行前体混合物的烘焙。包括镍,钴和锰的化合物以及锂化合物,从而制得锂复合氧化物。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号