PROBLEM TO BE SOLVED: To provide a method for producing a component using age hardening type bainitic non-heat treated steel, having high strength and low toughness.SOLUTION: The present invention provides a method for producing a component using age hardening type bainitic non-heat treated steel which contains, in mass%, C: 0.10-0.40%, Si: 0.01-2.00%, Mn: 0.10-3.00%, P: 0.001-0.150%, S: 0.001-0.200%, Cu: 0.001-2.00%, Ni: 0.40% or less, and Cr: 0.10-3.00%, and further contains one or more of Mo: 0.02-2.00%, V: 0.02-2.00%, Ti: 0.001-0.250%, and Nb: 0.010-0.100%, with the balance being Fe and unavoidable impurities, and the content (mass%) of the chemical components satisfying a predetermined relational expression, and the method including an age hardening step and a strain age hardening step.SELECTED DRAWING: Figure 1
机译:解决的问题:提供一种使用高强度低韧性的时效硬化型贝氏体非热处理钢制造零件的方法。解决方案:本发明提供一种使用时效硬化型贝氏体非热处理钢制造零件的方法。热处理钢,以质量%计包含C:0.10-0.40%,Si:0.01-2.00%,Mn:0.10-3.00%,P:0.001-0.150%,S:0.001-0.200%,Cu:0.001-2.00 %,Ni:0.40%以下,Cr:0.10〜3.00%,并且进一步含有Mo:0.02〜2.00%,V:0.02〜2.00%,Ti:0.001〜0.250%,Nb:0.010〜 0.100%,余量为Fe和不可避免的杂质,化学成分的含量(质量%)满足预定的关系式,该方法包括时效硬化步骤和应变时效硬化步骤。图1

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号