The invention relates to a multi-track laser beam process of surface hardening of steel sheet with low-carbon and low manganese steel. The resulting steel shows improved mechanical strength and can be used for manufacturing of automotive components. The process comprises the steps of: providing CRCA steel grades of ( low carbon and low manganese) in the form of flat sheet having a chemical composition range by weight percentage, C: 0.03-0.07, Mn: 0.15-0.25 and 1.4, S: 0.005-0.009, P: 0.009-0.014, Si: 0.005-0.02, Al: 0.04, V: 0.001, Nb: 0.001,and Ti:0.002; optimizing laser processing variables to reach austenizing temperature capable for phase transformation of the initial microstructure to harder dual phase structure of the steel sheet; selecting a laser track pattern for surface hardening of the steel sheet; applying the selected laser processing variables in the form of laser power (2.5-3.5 KW) - and scanning speed (150-250 mm/s) combinations on the surface of the steel sheet; selecting and adapting associated laser optics to operate the laser beam such that an impingement laser spot size on the sheet is of square shape, wherein a 6-axis robot employed to carry the laser through a fiber fixed on 6
机译:本发明涉及一种用低碳低锰钢对钢板进行表面硬化的多道激光束工艺。所得钢显示出改进的机械强度,并且可以用于制造汽车部件。该方法包括以下步骤:提供平板形式的CRCA钢种(低碳和低锰),其化学成分的重量百分比范围为C:0.03-0.07,Mn:0.15-0.25和1.4,S: 0.005-0.009,P:0.009-0.014,Si:0.005-0.02,Al:0.04,V:0.001,Nb:0.001,和Ti:0.002;优化激光加工变量以达到能够使钢板的初始微观结构相转变为较硬的双相结构的奥氏体温度;选择激光轨迹图案以对钢板进行表面硬化;在钢板表面上以激光功率(2.5-3.5 KW)和扫描速度(150-250 mm / s)组合的形式应用选定的激光加工变量;选择和调整相关的激光光学器件以操作激光束,以使薄片上的入射激光光斑尺寸为正方形,其中采用了6轴机械手来将激光传送通过固定在6层上的光纤

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号