The present invention relates to a method for manufacturing and constructing lightweight fire resistance foaming ceramic insulation for preventing fire spread on an exterior insulation layer of a building, which effectively inhibits the fire spread with respect to the exterior insulation layer of the building, never having been treated by a conventional fire protection facility, and prevents toxic gases from being generated, thereby being able to significantly enhance stability in fire. The present invention is based on a composition comprising: 75-95 wt% of glass sludge which is selected from one between waste glass powder and glass abrasive sludge or a mixture thereof; 1-20 wt% of an additive which is selected from one among fly ash, silica powder, waste concrete micropowder, stone powder and pearlite powder or a mixture made of two kinds or more thereof; 1-5 wt% of sodium silicate as a mixing and air entrainment additive; 0.1-5.0 wt% of an inorganic foaming agent selected from one among carbon black, calcium carbonate and magnesium carbonate or a mixture made of two kinds or more thereof in order to generate air bubbles at the temperature higher than a softening point of the glass sludge in a state of being surrounded by the glass sludge and then to form the air bubbles in the glass sludge in a state of being softened; and 1-10 wt% of a melting point lowering agent which is selected from one between boron and sodium carbonate or a mixture thereof in order to lower the melting point of the glass sludge.
机译:本发明涉及一种用于制造和构造轻质耐火泡沫陶瓷隔热材料的方法,该隔热材料用于防止火灾在建筑物的外墙保温层上蔓延,其有效地抑制了相对于建筑物外墙保温层的蔓延。通过常规消防设施进行处理,并防止产生有毒气体,从而能够显着提高火灾稳定性。本发明基于一种组合物,该组合物包含:75-95重量%的玻璃渣,其选自废玻璃粉和玻璃磨料渣或它们的混合物;和1-20重量%的添加剂,其选自粉煤灰,硅石粉,废混凝土微粉,石材粉和珠光体粉中的一种或两种以上的混合物; 1-5重量%的硅酸钠作为混合和引气添加剂;为了在高于玻璃泥的软化点的温度下产生气泡,从炭黑,碳酸钙和碳酸镁中的一种或两种或多种制成的混合物中选择0.1-5.0重量%的无机发泡剂。在被玻璃渣包围的状态下,然后以软化状态在玻璃渣中形成气泡。为了降低玻璃渣的熔点,从硼和碳酸钠中的一种或其混合物中选择1-10重量%的熔点降低剂。

著录项

  • 公开/公告号KR20180007646A

    专利类型

  • 公开/公告日2018-01-23

    原文格式PDF

  • 申请/专利号KR20160137647

  • 发明设计人 SONG HUN;SHIN HYEON UK;

    申请日2016-10-21

  • 分类号C04B18/30;C04B14/04;C04B14/06;C04B18/08;C04B18/16;C04B38/02;E04B1/76;

  • 国家 KR

  • 入库时间 2022-08-21 12:41:08

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号