The present invention provides a high elastic modulus fiberglass composition and glass fibers and composites thereof. The content of each component in the glass fiber composition is, in terms of weight percentage, 55.7-58.9% SiO 2, 15-19.9% Al 2 O 3, 0.1-4.3% Y 2 O 3 , La 2 O 3? 1.5%, CeO 2 ≤1.2%, CaO6-10%, MgO9.05-9.95% , SrO≤2%, O≤0.99% Li 2 O + Na 2 O + K 2, Li 2 O≤0.65%, Fe 2 O 3 1% , TiO 2 0.1-1.5%, and the ratio of the weight percentage of C 1 = Y 2 O 3 / (Y 2 O 3 + La 2 O 3 + CeO 2 ) is expressed as 0.6. This composition significantly improves the modulus of elasticity of the glass, significantly lowers the liquidus temperature and the molding temperature of the glass, greatly reduces the crystallization rate and the void ratio of the glass under the same conditions, and particularly reduces the glass transition temperature It is suitable for production.
机译:本发明提供了高弹性模量的玻璃纤维组合物和玻璃纤维及其复合材料。以重量百分比计,玻璃纤维组合物中的每种组分的含量为55.7-58.9%SiO 2, 15-19.9%Al 2 O 3 , 0.1-4.3%Y 2 O 3 ,La 2 O 3? 1.5%, CeO 2 ≤1.2%,CaO6-10%,MgO9.05-9.95%,SrO≤2%,O≤0.99%Li 2 O + Na 2 O + K 2,Li 2O≤0.65 %,Fe 2 O 3 <1%,TiO 2 0.1-1.5%,C 1的重量百分比= Y 2 O 3 < / Sub> /(Y 2 O 3 + La 2 O 3 + CeO 2 )表示为> 0.6。该组合物显着提高了玻璃的弹性模量,显着降低了液相线温度和玻璃的成型温度,在相同条件下大大降低了玻璃的结晶速率和空隙率,特别是降低了玻璃化转变温度。适合生产。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号