FIELD: construction.;SUBSTANCE: invention relates to road and airfield construction and can be used to stabilize and strengthen the soil during renovations, repairs, for the construction of additional base layers, bases and coatings with a wear layer of all types of pavements for areas with average monthly air temperature of the coldest month up to -30 °C. Composition for stabilization of natural and man-made soils contains, wt%: melanin 0.01–0.5, calcium formate 0.5–3.0, fly ash 1.0–8.0, sodium glass 0.01–1.0, sodium oleate 0.01–0.5, lignosulphonate technical LST 0.1–1.0, dolomite flour 0.5–3.0, salted lime 1.0–3.0, sodium ethyl silicate 0.01–0.5, active silica fume 0.01–0.1, sodium methylsiliconate 0.2–1.0, sodium, ammonium and iron sulfates 0.02–0.5, cement 78–96.63. Cement used is cement grade PC 500 D0 or CEM I 42.5N.;EFFECT: improving the quality of soil stabilization by reducing the possibility of the formation of shrinkage cracks in it, potholes and areas exposed to frost heaving, increasing the strength characteristics of the soil.;1 cl, 2 tbl
机译:技术领域本发明涉及道路和飞机场的构造,并且可以用于在翻新,修理期间稳定和加固土壤,用于构造用于所有类型的路面的附加基础层,基础和具有耐磨层的涂层。最冷月的平均每月气温不超过-30°C的地区。用于稳定天然和人造土壤的组合物,按重量百分比计:黑色素0.01-0.5,甲酸钙0.5-3.0,粉煤灰1.0-8.0,玻璃钠0.01-1.0,油酸钠0.01-0.5,木质素磺酸LST 0.1-1.0 ,白云石粉0.5-3.0,盐石灰1.0-3.0,硅酸乙酯钠0.01-0.5,活性硅粉0.01-0.1,甲基硅酸钠0.2-1.0,钠,铵和硫酸铁0.02-0.5,水泥78-96.63。所使用的水泥为PC 500 D0或CEM I 42.5N水泥等级;效果:通过减少在其中,坑洼处和冻胀处暴露的收缩裂缝的可能性来提高土壤稳定的质量,并提高水泥的强度特性。土壤。; 1厘升,2汤匙

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号