首页> 外国专利> METHOD OF PREPARING Ni-W CATALYST FOR HYDROCRACKING HYDROCARBON MATERIAL

METHOD OF PREPARING Ni-W CATALYST FOR HYDROCRACKING HYDROCARBON MATERIAL

机译:制备加氢裂化碳材料的镍钨催化剂的方法

摘要

FIELD: technological processes.;SUBSTANCE: invention relates to a method for preparing a catalyst for hydrocracking a hydrocarbon material by impregnating a calcined amorphous silica-alumina carrier with an aqueous solution obtained by mixing at a temperature of 90–95 °C in an aqueous solution of orthophosphoric acid 45–75 g/l, tungsten (III) oxide 290–460 g/l and nickel (II) carbonate 65–120 g/l, which is stabilized by a mixture of citric and oxalic acids with a concentration of 28–65 g/l with the formation of a stable water complex of active components, followed by drying the catalyst at 120–150 °C and further sulphidizing.;EFFECT: technical result consists in preparing a catalyst for the hydrocracking of hydrocarbon material with high activity and simplifying the process for its preparation.;4 cl, 3 tbl, 7 ex
机译:技术领域:本发明涉及一种通过将煅烧的无定形二氧化硅-氧化铝载体浸渍于在90-95℃的温度下在水溶液中混合而得的水溶液中来制备用于烃类材料加氢裂化的催化剂的方法。 45-75 g / l的正磷酸,290-460 g / l的氧化钨(III)和65-120 g / l的碳酸镍(II)的溶液,其浓度为柠檬酸和草酸的混合物28-65 g / l,形成稳定的活性成分水配合物,然后将催化剂在120-150°C下干燥并进一步硫化。效果:技术成果包括制备用于加氢裂化碳氢化合物的催化剂高活性并简化了制备过程。; 4 cl,3 tbl,7 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号