MASTER BATCH FOR POLYOLEFIN CROSSLINKED FOAM, POLYOLEFIN CROSSLINKED FOAM, AND MANUFACTURING METHOD OF POLYOLEFIN CROSSLINKED FOAM

机译:聚烯烃交联泡沫的主批料,聚烯烃交联泡沫和聚烯烃交联泡沫的制造方法

摘要

To provide a polyolefin crosslinked foam low in remaining ammonium concentration, capable of preventing contamination or corrosion due to ammonia, and suitable for impact cushioning applications such as a floor material or a wall material of house, a joint filling material of building, an automotive interior member, a member for package or the like.SOLUTION: There is provided a polyolefin crosslinked foam having density of 20 to 160 kg/m, ammonia concentration of 0 ppm to 100 ppm, and glass haze degree of 5% or less, obtained by a mixed article containing a master batch for polyolefin crosslinked foam containing an ethylene vinyl acetate copolymer with vinyl acetate content of 18 wt.% or more and/or an ethylene-propylene-diene three dimensional copolymer with Mooney viscosity (ML1+4, 100°C) of 20 to 40, and sodium bicarbonate and p,p'-oxybisbenzenesulfonyl hydrazide as foaming agents, a polyolefin resin, and a crosslinking agent.SELECTED DRAWING: Figure 1
机译:为了提供残留铵浓度低的聚烯烃交联泡沫,能够防止由于氨引起的污染或腐蚀,并且适合于冲击缓冲应用,例如房屋的地板材料或墙壁材料,建筑物的接缝填充材料,汽车内部解决方案:提供一种通过以下方法得到的聚烯烃交联泡沫,其密度为20至160 kg / m,氨气浓度为0 ppm至100 ppm,玻璃雾度为5%以下。包含用于聚烯烃交联泡沫的母料的混合制品,所述母料包含乙酸乙烯酯含量为18wt。%或更高的乙烯乙酸乙烯酯共聚物和/或门尼粘度为(ML1 + 4,100°的乙烯-丙烯-二烯三维共聚物C)20至40,以及碳酸氢钠和p,p'-氧基双苯磺酰肼作为发泡剂,聚烯烃树脂和交联剂。图1

著录项

  • 公开/公告号JP2019131703A

    专利类型

  • 公开/公告日2019-08-08

    原文格式PDF

  • 申请/专利权人 INOAC CORP;

    申请/专利号JP20180014713

  • 发明设计人 NAKANO SUSUMU;HASHIMOTO NAOKI;

    申请日2018-01-31

  • 分类号C08J9/06;C08J3/22;

  • 国家 JP

  • 入库时间 2022-08-21 12:23:14

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号