To provide an electromagnetic steel that suppresses decrease in magnetic flux density during annealing for removing distortions and a method of producing the same.SOLUTION: An electromagnetic steel contains Si of 2.0 mass% or more and 4.5 mass% or less and Mn of 2.5 mass% or more and 5.0% mass or less, and further contains at least one element selected from Ca, Mg, Ce, Ti, Ba, and Be in a total of 0.0001 mass% or more and 0.1 mass% or less, with Al of less than 0.03 mass%, C of less than 0.002 mass%, and S of less than 0.002 mass%, the steel having Fe as the main component. The steel has an average crystal grain size of 60 μm or more and 80 μm or less.SELECTED DRAWING: Figure 1
机译:提供一种抑制退火中的磁通密度降低以消除变形的电磁钢及其制造方法。解决方案:电磁钢包含2.0质量%以上且4.5质量%以下的Si和2.5质量%的Mn。大于或等于5.0质量%以下,并且进一步包含选自Ca,Mg,Ce,Ti,Ba和Be中的至少一种元素,其总量为0.0001质量%以上且0.1质量%以下,且Al小于以Fe为主要成分的钢小于0.03质量%,C小于0.002质量%,S小于0.002质量%。该钢的平均晶粒尺寸为60μm以上且80μm以下。

著录项

  • 公开/公告号JP2019019355A

    专利类型

  • 公开/公告日2019-02-07

    原文格式PDF

  • 申请/专利权人 NIPPON STEEL & SUMITOMO METAL;

    申请/专利号JP20170137275

  • 发明设计人 TOMITA MIHO;FUJIMURA HIROSHI;

    申请日2017-07-13

  • 分类号C22C38;C22C38/14;C21D8/12;H01F1/147;C22C38/60;

  • 国家 JP

  • 入库时间 2022-08-21 12:20:29

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号