Electrodeposited copper foil having optimized peak roughness, electrode containing the same, secondary battery containing the same, and method of manufacturing the same

机译:具有最佳峰粗糙度的电沉积铜箔,包含该铜箔的电极,包含该铜箔的二次电池及其制造方法

摘要

Provided is an electrolytic copper foil, an electrode including the same, a secondary battery including the same, and a method of manufacturing the same. The electrolytic copper foil has an optimizedpeak roughness so as to improve a capacity retention ratio of the secondary battery. The electrolytic copper foil includes a first surface and a second surface opposite to the first surface, wherein each of the first surface and the second surface has a peak roughness (Rp) of 0.36 microns to 1.69 microns, and The difference between the peak roughness (Rp) of one surface and the peak roughness (Rp)of the second surface is 0.6 microns or less.
机译:提供一种电解铜箔,包括该电解铜箔的电极,包括该电解铜箔的二次电池及其制造方法。电解铜箔具有最佳的峰粗糙度,从而提高了二次电池的容量保持率。电解铜箔包括第一表面和与第一表面相对的第二表面,其中第一表面和第二表面中的每一个具有0.36微米至1.69微米的峰粗糙度(Rp),并且峰粗糙度之间的差为一个表面的Rp)和第二表面的峰值粗糙度(Rp)为0.6微米或更小。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号