Provided are a polyurethane-modified epoxy resin composition having satisfactory operability of processing, such as casting or impregnation, in a composition state, a production method therefor, and a composition thereof. The polyurethane-modified epoxy resin is obtained by modifying a secondary hydroxyl group-containing bisphenol-based epoxy resin (a) having an epoxy equivalent from 150 g/eq to 200 g/eq and a hydroxyl equivalent from 2,000 g/eq to 2,600 g/eq with a polyol compound (b) having an Mn of 200 or more, a polyisocyanate compound (c), and a polyol compound (d) having an Mn of less than 200 serving as a chain extender. The polyurethane-modified epoxy resin uses the epoxy resin (a) in an amount from 20 wt % to 60 wt % with respect to the total amount of the respective components (a), (b), (c), and (d), and contains a polyurethane having the epoxy resin (a) added to both terminals thereof and/or one terminal thereof.
机译:本发明提供了一种在组合物状态下具有令人满意的加工性例如浇铸或浸渍的聚氨酯改性环氧树脂组合物,其制备方法及其组合物。通过将环氧当量为150g / eq至200g / eq和羟基当量为2,000g / eq至2,600g的含仲羟基的双酚类环氧树脂(a)进行改性而获得聚氨酯改性的环氧树脂。 Mn为200以上的多元醇化合物(b),多异氰酸酯化合物(c)和Mn为小于200的多元醇化合物(d)为扩链剂。相对于各组分(a),(b),(c)和(d)的总量,聚氨酯改性的环氧树脂以20重量%至60重量%的量使用环氧树脂。并包含聚氨酯,该聚氨酯具有在其两个末端和/或其一个末端上添加的环氧树脂(a)。

著录项

  • 公开/公告号US10266637B2

    专利类型

  • 公开/公告日2019-04-23

    原文格式PDF

  • 申请/专利权人 NIPPON STEEL & SUMIKIN CHEMICAL CO. LTD.;

    申请/专利号US201515315215

  • 申请日2015-06-02

  • 分类号C08G18/58;C08G59/14;C08G59/22;C08G18/12;C08G18/76;C08G59/42;C08L63;C08L75/08;C08G18/48;C08G18/64;C08G59/40;C08G59/20;C08G18/66;C08G18/40;

  • 国家 US

  • 入库时间 2022-08-21 12:14:45

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号