摘要

A method of preparing a three-dimensional composite material includes the following steps: preparing polystyrene by soap-free emulsion polymerizing, obtaining polystyrene opal by a vertical deposition method, synthesizing MoP IO (molybdenum phosphide inverse opal), and compounding with quantum points CdS, so as to obtain a novel inorganic composite material, namely cadmium sulfide quantum dot-compounded MoP IO. The preparation method has the advantages that the MoP IO is prepared first, and the MoP IO is of a three-dimensional cyclic pore structure and has the photonic band gap feature, so that the MoP IO has better catalysis effect in light catalysis in comparison with that of common porous material; the MoP IO is compounded with the cadmium sulfide quantum dots, so that the light absorbing ability is enhanced, and the composite material capable of absorbing the visible light is obtained.
机译:制备三维复合材料的方法包括以下步骤:通过无皂乳液聚合制备聚苯乙烯;通过垂直沉积法获得聚苯乙烯蛋白石;合成MoP IO(磷化钼反相蛋白石);以及与量子点CdS混合,从而获得一种新型的无机复合材料,即硫化镉量子点复合MoP IO。该制备方法的优点是,首先制备了MoP IO,且MoP IO具有三维环状孔结构,并具有光子带隙特征,因此与光催化相比,MoP IO在光催化方面具有更好的催化效果。普通多孔材料的MoP IO与硫化镉量子点复合,提高了光吸收能力,得到了能够吸收可见光的复合材料。

著录项

  • 公开/公告号US2019329233A1

    专利类型

  • 公开/公告日2019-10-31

    原文格式PDF

  • 申请/专利权人 SOOCHOW UNIVERSITY;

    申请/专利号US201916396607

  • 发明设计人 JIANMEI LU;NAJUN LI;

    申请日2019-04-26

  • 分类号B01J35;B01J27/19;B01J37/04;B01J37/08;B01J37;B01J37/06;B01J37/32;C02F1/30;

  • 国家 US

  • 入库时间 2022-08-21 12:10:17

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号