process to obtain a transplant to regenerate bone tissue, especially human, characterised by the fact that consists of the following steps: cleaning mechanical bones broken, encephalopathy or korowo - encephalopathy, preferably of human origin with soft tissue, and was eleni bone fragments, favourably degreasing bone in c2h5oh concentration from 60% to 96%.degreasing bone in h2o2 concentration from 1% to 40%, at least once rinsing bone in nacl at concentrations from 0.1% to 10%, doczyszczania mechanical bones, bones from the remnants of the draining nacl, freezing bone in the temp.around - 105, bone grinding mill operated until granules, granules by screening system in order to sit, of appropriate fractions, positive granules in the freezing temp. around - 105 and sterilization radiacyjnej granules, preferably of 35 kgy.transplant to regenerate bone tissue, especially human, characterised by the fact that it is a spongy bone tissue, korowo - or spongy, preferably of human origin, in the form of pellets, purified mechanically with the soft tissue, divided into fragments, preferably odu0142u szczana in c2h5oh concentration from 60% to 96%, odtu0142uszczana in h2o2 concentration from 1% to 40%.at least once washed in nacl at concentrations from 0.1% to 10%, doczyszczona mechanically, without residual nacl, h2o2, advantageously also c2h5oh, frozen in the temp. around - 105, ground to obtain granules, sieved by the system in order to sit, of appropriate fractions favourably again frozen in the temp. approximately 100 degrees and sterilised radiacyjnie, advantageously in a dose of 35 kgy.
机译:一种获得移植物以再生骨骼组织,特别是人体的方法,其特征在于以下步骤组成的事实:用软组织清洁破裂的机械性骨骼,脑病或颅脑病,最好是人源性的,并且是柔软的骨碎片将c2h5oh浓度中的骨骼脱脂从60%降至96%。将h2o2浓度中的骨骼脱脂从1%至40%,至少一次以0.1%到10%的浓度在Nacl中冲洗骨骼,doczyszczania机械骨骼,来自骨骼残余的骨骼在105左右的温度下排干氯化钠,冷冻骨头,直到通过筛分系统运转颗粒直至颗粒,颗粒,以便将适当量的阳性颗粒静置在冷冻温度下。大约-105毫米的放射状杀菌颗粒,最好是35公斤/千克的放射状杀菌颗粒,用于再生骨骼组织,特别是人类的骨骼,其特征在于,它是一种海绵状的骨组织,呈球形或海绵状,最好是人类来源的,呈颗粒状,用软组织机械纯化,分成碎片,优选c2h5oh浓度从60%到96%的odz,h2o2浓度从1%到40%的odz至少一次在nacl中以0.1%的浓度洗涤在室温下冷冻至10%,机械地doczyszczona,没有残留的氯化钠,h2o2,有利地还有c2h5oh。大约在-105℃下,研磨以得到颗粒,然后将其通过系统过筛以静置,并适当地再次冷冻。大约100度,并以35 kgy的剂量灭菌后的radiacyjnie。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号