首页> 外国专利> Improved method for the treatment of tobacco ribs and /or ribs.

Improved method for the treatment of tobacco ribs and /or ribs.

机译:治疗烟草和/或肋骨的改进方法。

摘要

An improved method for treating, preferably by the expansion treatment, the stems of tobacco and/or leaf veins (1) of tobacco, in particular those discarded by cigarette making machines,providing the sequence of the following steps: - a step (2) of moistening said stems and/or leaf veins (1) such that said stems and/or leaf veins (1) have a moisture at the end of said step, which is measured on moisture basis, ranging from 35 to 85% and a volume which is greater than the initial volume thereof before said moistening step (2), - at least one laminating step (4) of said previously moistened stems and/or leaf veins (1), such that the stems and/or the leaf veins have a thickness ranging from 0.07 to 1.7 mm at the end of the laminating, - at least one drying step (5) of said previously moistened and laminated stems and/or leaf veins (1), such that said stems and/or leaf veins (1) have a moisture ranging from 20 to 40% at the end of said step, and bcharacterized in that/b : - said at least one laminating step (4) is carried out immediately after said moistening step (2), - said at least one drying step (5) is carried out immediately after said at least one laminating step (4).
机译:一种改进的方法,最好通过膨胀处理来处理烟草的茎杆和/或烟草的叶脉(1),特别是由制烟机丢弃的那些,提供以下步骤的顺序:-步骤(2)润湿所述茎和/或叶脉(1),以使所述茎和/或叶脉(1)在所述步骤结束时具有水分,该水分以水分为基础测量,范围为35%至85%其大于所述润湿步骤(2)之前的初始体积,-所述先前润湿的茎和/或叶脉(1)的至少一个层压步骤(4),使得茎和/或叶脉具有在层压结束时的厚度范围为0.07至1.7毫米;-至少对上述先前润湿和层压的茎和/或叶脉(1)进行干燥步骤(5),以使所述茎和/或叶脉( 1)在所述步骤结束时的水分含量在20%至40%之间,并且其特征在于:-在在所述润湿步骤(2)之后立即进行一个层压步骤(4),-在所述至少一个层压步骤(4)之后立即进行所述至少一个干燥步骤(5)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有