The present invention relates to a quartz glass fiber-containing prepreg, comprising (A) a quartz glass fiber and (B) a curable resin composition, wherein at least one of the following conditions is met: (1) the quartz glass fiber contains an α-ray level of 0.005c/cm^2·hr or less, and contains 1 ppm or less of each of metal ions, Na^+, Li^+, and K^+; (2) the number of pores in the quartz glass fiber is 10 or less per unit surface area, m^2; and (3) the quartz glass fiber-containing prepreg has a tolerant flexural strength of 500 N·m^2 or higher when the thickness as measured by a method described in JIS R 3420:2013 is 100-200 μm. Accordingly, the present invention may provide a quartz glass fiber-containing prepreg having excellent dielectric properties, excellent thermal resistance, and/or excellent handling properties due to high flexural strength.
机译:本发明涉及一种含石英玻璃纤维的预浸料,其包括(A)石英玻璃纤维和(B)可固化树脂组合物,其中满足以下条件中的至少一个:(1)石英玻璃纤维包含可固化的树脂。 α射线水平为0.005c / cm ^ 2·hr或更小,并且包含1ppm以下的金属离子Na ^ +,Li ^ +和K ^ +; (2)石英玻璃纤维中的细孔数为每单位表面积10个以下,m ^ 2。 (3)当通过JIS R 3420:2013中记载的方法测定的厚度为100〜200μm时,含有石英玻璃纤维的预浸料的耐弯曲强度为500N·m ^ 2以上。因此,本发明可以提供由于高的弯曲强度而具有优异的介电性能,优异的耐热性和/或优异的操作性的含石英玻璃纤维的预浸料。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号