FIELD: metallurgy.SUBSTANCE: invention can be used in the preparation of raw materials for the iron and steel industry. For the utilization of chromium slime sludge, joint processing of chromium slime with iron ore concentrate is carried out during the agglomeration of the charge. Thermal treatment of the sludge is carried out in the temperature range 1100–1400 °C. As starting components of the charge, a chromate slurry is used, iron ore concentrate and coke at the following ratio of dry weight components, by weight: iron ore concentrate 63–71, chromate slurry 21–31, coke 6–8.EFFECT: invention makes it possible to convert hexavalent chromium to a safe state by combining the processing of slimes of chromate production with iron ore concentrate during the agglomeration of the charge and subsequent smelting of cast iron, simplify the process of neutralization and processing of sludge by involving it in the technological processes of ferrous metallurgy, while waste of chromate production is added to agglomerate instead of traditional fluxing additives such as limestone.1 cl, 1 tbl
机译:领域:冶金。物质:发明可用于钢铁工业的原料制备。为了利用铬泥污泥,在装料附聚过程中进行了铬泥与铁精矿的联合处理。污泥的热处理在1100–1400°C的温度范围内进行。作为进料的起始成分,使用铬酸盐浆,铁精矿和焦炭,其重量比如下:铁精矿63-71,铬酸盐浆21-31,焦炭6-8。本发明通过在装料的附聚和随后的铸铁熔炼中结合铬酸盐生产泥和铁矿石精矿的处理,将六价铬转化为安全状态成为可能,从而简化了中和过程和污泥的处理。在黑色冶金的工艺过程中,将铬酸盐生产废料添加到团聚体中,而不是传统的助熔添加剂(例如石灰石)。1cl,1 tbl

著录项

  • 公开/公告号RU2017117792A3

    专利类型

  • 公开/公告日2018-11-23

    原文格式PDF

  • 申请/专利权人

    申请/专利号RU20170117792

  • 发明设计人

    申请日0000-00-00

  • 分类号C22B1/16;C01G37;B09B3;C22B7;C22C37/06;C22C33/08;C21B3/06;

  • 国家 RU

  • 入库时间 2022-08-21 11:47:12

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号