FIELD: metallurgy.;SUBSTANCE: invention relates to a method for arc welding in a protective gas medium of two steel sheets using a welding torch with a consumable electrode. Protective gas having an oxygen potential is supplied from welding torch to consumable electrode α, which is from 1.5 to 5 %, which is determined from given expression depending on the proportion of inert gas, oxygen and carbon dioxide included in protective gas. Oxidising gas having oxygen potential is blown β, which ranges from 15 to 50 %, which is determined from a given expression depending on the ratio of the inert gas, oxygen and carbon dioxide contained in the oxidising gas. At that, rate of oxidising gas flow is from 1 to 3 m/s above welding bead and fifth welded joint, surface temperature of which is 700 °C or higher.;EFFECT: method makes it possible to form welded joint of structural elements with high corrosion resistance due to regulation of slag composition at welded seam.;7 cl, 8 dwg, 4 tbl
机译:用于具有可消耗电极的焊炬在两张钢板的保护性气体介质中进行电弧焊的方法技术领域本发明涉及一种使用具有可消耗电极的焊炬在两张钢板的保护性气体介质中进行电弧焊的方法。从焊炬向消耗电极α提供具有氧气电势的保护气体,该保护气体的量为1.5%至5%,这取决于给定表达式,具体取决于保护气体中所含惰性气体,氧气和二氧化碳的比例。吹入具有氧势的氧化气体,其范围为15%到50%,这取决于给定表达式,具体取决于氧化气体中所含惰性气体,氧气和二氧化碳的比例。那时,氧化气流的速度比焊缝和表面温度为700°C或更高的第五焊接接头高1至3 m / s;效果:方法使得可以用以下方法形成结构元件的焊接接头:由于调节了焊缝的熔渣成分,因此具有很高的耐腐蚀性; 7 cl,8 dwg,4 tbl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号