PROBLEM TO BE SOLVED: To provide a slag having excellent boron elution resistance, a method for producing the slag, and a civil engineering material using the slag. SOLUTION: With the glass phase As the crystal phase, at least Ca 3 Mg (SiO 4 ) 2 and B: 0.15% by mass or more, A slag containing Ba: 1.0% by mass or more and less than 2.5% by mass, and / or Sr: 0.40% by mass or more and less than 1.7% by mass. The following Index G obtained by XRD measurement using Cu-Kα ray as a radiation source is 7.0 or more. A slag having an excellent boron elution resistance, having a Ba content of less than 8.0% by mass and an Sr content of less than 7.0% by mass in the glass phase. Index G = I [glass] / (I [27 °] + I [32 °] + I [47 °]) x 100 [Selection diagram] None
机译:解决的问题:提供具有优异的耐硼溶出性的炉渣,该炉渣的制造方法以及使用该炉渣的土木工程材料。解决方案:以玻璃相作为晶相,至少Ca 3 Mg(SiO 4 2 和B:0.15%质量或含有Ba:1.0质量%以上且小于2.5质量%,和/或Sr:0.40质量%以上且小于1.7质量%的炉渣。通过使用Cu-Kα射线作为放射线源的XRD测量获得的以下指数G为7.0以上。一种具有优异的耐硼溶出性的炉渣,其在玻璃相中的Ba含量小于8.0质量%,并且Sr含量小于7.0质量%。索引G = I [玻璃] /(I [27°] + I [32°] + I [47°])x 100 [选择图]无

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号