the object of the application is the way of niskotarciowych and przeciwzuu017cyciowych ceramic coatings tlenkowych containing molybdenum disulfide, on the surface of metal materials.ceramic and polymer, which is thatthe coating material is prepared by dispersion of molybdenum disulphide powder structure heksagonalnej in zolu metal oxide or pu00f3u0142metalu in water or alcohol,with the possible addition of dysperguju0105cego, at room temperature.the reconstituted suspension in zolu molybdenum disulphide, metal oxide or pu00f3u0142metalu inscribed on the surface modified substrate at room temperature.after the substrate with coating made first dried at room temperature in 5 - 30 minutes.and then warm in temperature dependent on the type of zolu and material substrate in time also dependent on the type of zolu and substrate material.
机译:本申请的目的是在金属和金属材料的表面上使用含二硫化钼的niskotarciowych和przeciwzu u017cyciowych陶瓷涂料tlenkowych的方法,即陶瓷和聚合物,该涂料是通过将二硫化钼粉末结构heksagonalnej分散在zolu金属中而制得的在室温下,可以在水中或乙醇中加入dysperguj u0105cego的氧化物或金属氧化物。在室温下,表面改性的底材上刻有二硫化二氧化钼,金属氧化物或p u00f3金属的重构悬浮液。在制成带涂层的基材之后,首先在室温下干燥5-30分钟,然后根据zolu和材料基材的温度加热,时间又取决于zolu和基材材料的类型。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号