PROCESS FOR OBTAINING SIZE-CALIBRATED TRI-CALCIUM ALUMINATE PARTICLES AND USE OF SUCH PARTICLES IN A PROCESS OF ALUMINA REFINING

机译:在氧化铝精炼过程中获得尺寸标定的铝酸三钙颗粒的过程以及此类颗粒的使用

摘要

The present invention describes a process for obtaining size-calibrated tri-calcium aluminate (TCA) particles comprising the steps of providing a process liquor containing sodium aluminate; providing a suspension of size-calibrated calcium hydroxide particles; mixing said selected suspension of size-calibrated calcium hydroxide particles with said process liquor to allow them to react to obtain the said size-calibrated tri-calcium aluminate particles.
机译:本发明描述了一种获得尺寸校准的铝酸三钙(TCA)颗粒的方法,该方法包括以下步骤:提供一种含有铝酸钠的加工液。提供尺寸校准过的氢氧化钙颗粒的悬浮液;将所述选择的尺寸校准的氢氧化钙颗粒的悬浮液与所述处理液混合,以使它们反应以获得所述尺寸校准的铝酸三钙颗粒。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号