首页> 外国专利> PROCESS FOR OBTAINING SIZE-CALIBRATED TRI-CALCIUM ALUMINATE PARTICLES AND USE OF SUCH PARTICLES IN A PROCESS OF ALUMINA REFINING

PROCESS FOR OBTAINING SIZE-CALIBRATED TRI-CALCIUM ALUMINATE PARTICLES AND USE OF SUCH PARTICLES IN A PROCESS OF ALUMINA REFINING

机译:获得尺寸校准三钙铝酸钙颗粒的方法,并在氧化铝精炼过程中使用这种颗粒

摘要

The present invention describes a process for obtaining size-calibrated tri-calcium aluminate (TCA) particles comprising the steps of providing a process liquor containing sodium aluminate; providing a suspension of size-calibrated calcium hydroxide particles; mixing said selected suspension of size-calibrated calcium hydroxide particles with said process liquor to allow them to react to obtain the said size-calibrated tri-calcium aluminate particles.
机译:本发明描述了获得尺寸校准的三钙铝酸铝(TCA)颗粒的方法,包括提供含铝酸钠的工艺液体的步骤;提供悬浮型尺寸校准的氢氧化钙颗粒;将所述选定的悬浮液与所述液体液体混合,使它们使它们反应以获得所述尺寸校准的三钙铝酸钙颗粒。