To reduce the toxicity and achieve a sustainable and controllable release of cisplatin (CDDP).CDDP was loaded onto Fe5 (Fe(3+) doped hydroxyapatite at atomic ratio of Fe(added)/Ca(added)?=?5%) nanoparticles through surface adsorption. Subsequently, CDDP-loaded Fe5 nanoparticles (CDDP-Fe5) and/or CDDP were encapsulated into poly(lactide-co-glycolide) (PLGA) microspheres using oil-in-water single emulsion. Drug release profiles and degradation behaviors were monitored.CDDP-Fe5 demonstrated a high initial burst (42% on day 1) and short release time (25?days) as CDDP was directly released from Fe5 nanoparticles. CDDP-Fe5 encapsulated within the PLGA microspheres revealed a lower initial burst (23% on day 1) and longer release time (55?days) than CDDP-Fe5. Compared with PLGA microspheres containing only CDDP, which showed typical biphasic release manner, microspheres with CDDP-Fe5 and CDDP demonstrated a nearly linear release after the initial burst. Fe5 and CDDP delayed microsphere degradation. All samples became porous, disintegrated, fused, and formed pellets at the end of the study.Fe5/PLGA composite microspheres showed favorable CDDP release behavior compared to microspheres composed of polymer alone, suggesting its potential as a new CDDP formulation.
机译:为了降低毒性并实现顺铂(CDDP)的可持续和可控释放。将CDDP负载在Fe5(Fe(3+)掺杂的羟基磷灰石上,原子比为Fe(添加)/ Ca(添加)?=?5%)通过表面吸附。随后,使用水包油单乳液将负载CDDP的Fe5纳米颗粒(CDDP-Fe5)和/或CDDP封装到聚丙交酯-乙交酯共聚物(PLGA)微球中。监测药物的释放曲线和降解行为。由于CDDP是直接从Fe5纳米颗粒中释放出来的,因此CDDP-Fe5表现出较高的初始爆发(第1天为42%)和较短的释放时间(25天)。封装在PLGA微球中的CDDP-Fe5与CDDP-Fe5相比,显示出较低的初始爆发(第1天为23%)和更长的释放时间(55天)。与仅包含CDDP的PLGA微球相比,PLGA微球具有典型的双相释放方式,而具有CDDP-Fe5和CDDP的微球在初次爆发后表现出几乎线性的释放。 Fe5和CDDP延迟了微球的降解。在研究结束时,所有样品均变为多孔,崩解,熔融并形成颗粒。与仅由聚合物组成的微球相比,Fe5 / PLGA复合微球显示出良好的CDDP释放性能,表明其具有作为新型CDDP制剂的潜力。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号