Ancient ceramics from the archaeological site of Ebla (Syria), dating back between 2250 and 1800 B.C., have been characterized by a combined use of optical microscopy (OM), X-ray powder diffraction (XRPD) and micro-Raman spectroscopy (micro-RS). Petrographic observations indicate that different fabrics are present, in terms of microstructure, groundmass and inclusions. XRPD allowed the identification and quantification of mineral phases of both unheated and heated samples at 950 °C, by means of Rietveld refinements. In particular, XRPD of heated samples highlights significant differences among the mineralogical assemblages of the analyzed samples, suggesting that the relative amount of carbonate and silicate minerals plays a key role, driving the reactions during the firing process. Furthermore, the mineralogical composition of unheated samples suggests a firing temperature in the 800-850 °C range, excluding a sample fired at lower temperatures (400-500 °C). Concerning the redox state of the firing atmosphere, the occurrence of hematite in some samples indicates that they were fired in oxidizing conditions, whereas other ceramic artifacts containing magnetite were fired in reducing conditions. Micro-RS results highlight that the mineralogical components of the decorated surfaces are hematite in the red areas and magnetite in the black ones.
机译:埃布拉(叙利亚)考古遗址的古代陶瓷可追溯到公元前2250年至1800年,其特征是结合使用光学显微镜(OM),X射线粉末衍射(XRPD)和显微拉曼光谱法(micro-Raman RS)。岩石学观察表明,就微观结构,基础质量和包裹体而言,存在着不同的织物。 XRPD可以通过Rietveld精炼技术鉴定和定量950°C下未加热和加热样品的矿物相。特别地,加热样品的XRPD突出显示了所分析样品的矿物学组成之间的显着差异,这表明碳酸盐和硅酸盐矿物的相对含量起着关键作用,在焙烧过程中驱动反应。此外,未加热样品的矿物学组成表明烧结温度在800-850°C范围内,不包括在较低温度(400-500°C)下燃烧的样品。关于烧成气氛的氧化还原状态,一些样品中赤铁矿的出现表明它们在氧化条件下烧成,而其他含磁铁矿的陶瓷制品在还原条件下烧成。 Micro-RS结果表明,装饰表面的矿物成分是红色区域的赤铁矿和黑色区域的磁铁矿。

著录项

相似文献

  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号