Poly(methyl methacrylate)/polyethyleneimine (PMMA/PEI) core-shell nanoparticles were prepared by emulsifier free emulsion polymerization. Micrographs from a scanning electron microscope and transmission electron microscope displayed their spherical shape with core-shell morphology in which PMMA was a core and PEI was a shell. The PMMA/PEI nanoparticles' ability to adsorb proteins from the serum of commercial low-ammonia preserved fresh field natural rubber latex was illustrated. The driving force for adsorption was proposed to be mainly via electrostatic interaction between the protonated amino groups of PEI chains on the nanoparticles' surface and phospholipids or protein molecules on NR particles. The reduction percentage was about 50%, depending on the content of PMMA/PEI nanoparticles and mixing time. For comparison, the protein reduction performance by the nanoparticles with two additional extracted serums, high-ammonia preserved concentrated NRL and Thai advanced preservative system NRL, which have different initial protein contents and pH values, was also investigated. The preliminary evaluation of PMMA/PEI nanoparticles' performance in sulfur-prevulcanized high-ammonia preserved concentrated NRL was also studied. Its corresponding sheet had lower extractable proteins by 50% and had tensile strength and elongation at break of 25.5 MPa and 715%, respectively.
机译:聚(甲基丙烯酸甲酯)/聚乙烯亚胺(PMMA / PEI)核壳纳米粒子是通过无乳化剂乳液聚合制备的。来自扫描电子显微镜和透射电子显微镜的显微照片显示它们的球形,具有核-壳形态,其中PMMA为核,PEI为壳。说明了PMMA / PEI纳米颗粒从商业低氨气保存的新鲜田间天然胶乳的血清中吸附蛋白质的能力。提出吸附的驱动力主要是通过纳米颗粒表面上PEI链的质子化氨基与NR颗粒上的磷脂或蛋白质分子之间的静电相互作用。还原百分率约为50%,具体取决于PMMA / PEI纳米颗粒的含量和混合时间。为了进行比较,还研究了具有另外两种提取血清的纳米颗粒的蛋白质还原性能,这两种血清分别具有不同的初始蛋白质含量和pH值,分别是高氨保存的浓缩NRL和Thai高级防腐剂系统NRL。还研究了PMMA / PEI纳米颗粒在硫磺硫化高氨气保存的浓缩NRL中的性能的初步评估。其相应的片具有较低的可提取蛋白质50%,并且具有抗张强度和断裂伸长率分别为25.5MPa和715%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号