Preparation and characterization of a dialdehyde starch crosslinked feather keratin film for food packaging application

机译:食品包装用二醛淀粉交联羽毛角蛋白薄膜的制备与表征

获取原文
获取原文并翻译 | 示例
           

摘要

Feathers, a byproduct of the poultry industry, have long been considered as a solid waste, posing a series of environmental and economic problems. However, feather keratin (FK) extracted from feathers is a valuable source of the biodegradable and biocompatible polymer. The aim of this study was to develop and characterize novel casting films based on feather keratin (FK) crosslinked by dialdehyde starch (DAS) and plasticized with glycerol for applications in biomedicine. The microstructure, crystallization behavior, light transmission, moisture content, solubility, tensile properties, water vapor barrier property, and cytotoxicity of the FK-DAS films were investigated. The fracture surface of the crosslinked film showed a more compact microstructure than that of the control film, and the crosslinked films were completely amorphous and very transparent (transparency value <2). These results indicate that the addition of DAS increased the transparency value and moisture content and decreased the solubility, indicating the crosslinking between the FK and DAS. The films with 2% DAS showed increased tensile elongation and water vapor permeability compared to the control films, whereas the tensile strength of the film decreased, most probably because the crosslinking effect was counterbalanced by the plasticization of DAS. DAS increased the water resistance of the FK films, thus expanding their potential application in food packaging.
机译:禽类工业的副产品羽毛长期以来一直被视为固体废物,带来了一系列环境和经济问题。但是,从羽毛中提取的羽毛角蛋白(FK)是可生物降解和生物相容性聚合物的重要来源。这项研究的目的是开发和表征基于羽化角蛋白(FK)的新型流延膜,该流延膜通过二醛淀粉(DAS)交联并用甘油增塑,用于生物医学。研究了FK-DAS薄膜的微观结构,结晶行为,透光性,水分含量,溶解度,拉伸性能,水蒸气阻隔性能和细胞毒性。交联膜的断裂表面显示出比对照膜更紧密的微观结构,并且交联膜完全无定形且非常透明(透明度值<2)。这些结果表明,DAS的添加增加了透明度值和水分含量并且降低了溶解度,表明FK和DAS之间的交联。与对照薄膜相比,具有2%DAS的薄膜显示出更高的拉伸伸长率和水蒸气渗透性,而薄膜的拉伸强度却下降了,这很可能是因为DAS的增塑作用抵消了交联效果。 DAS增强了FK薄膜的耐水性,从而扩大了其在食品包装中的潜在应用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号