Monodisperse Ru-B amorphous alloy catalysts were synthesized by ultrasound-assisted chemical reduction of (NH4)(2)RuCl6 with BH (4) (-) . With the characterization of X-ray diffraction (XRD), selective area electronic diffraction (SAED), X-ray photoelectron spectroscopy (XPS), differential scanning calorimetry (DSC), and transmission electron microscopy (TEM), the resulting Ru-B nanoparticles were identified to be amorphous alloys ranging in size from 2.4 to 4.9 nm. During liquid-phase maltose hydrogenation, the as-synthesized Ru-B catalyst was extremely active compared to the regular Ru-B obtained via the reduction of RuCl3 with BH (4) (-) . The Ru-B sample prepared under ultrasonication with 60 W was proven to be the most active catalyst. Its catalytic activity was nearly 11 times that of industrial Raney Ni, and could be used repetitively for more than six times without significant deactivation.
机译:通过BH(4)(-)的超声辅助化学还原(NH4)(2)RuCl6合成了单分散Ru-B非晶态合金催化剂。通过X射线衍射(XRD),选择性区域电子衍射(SAED),X射线光电子能谱(XPS),差示扫描量热法(DSC)和透射电子显微镜(TEM)的表征,得到了Ru-B纳米粒子经鉴定为非晶态合金,尺寸范围为2.4至4.9 nm。在液相麦芽糖加氢过程中,与通过BH(4)(-)还原RuCl3获得的常规Ru-B相比,合成后的Ru-B催化剂具有极高的活性。经证实,在60 W的超声波作用下制备的Ru-B样品是活性最高的催化剂。它的催化活性是工业阮内镍的近11倍,可以重复使用六次以上而不会明显失活。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号