Possibilities of a Thermomechanical Method for Enriching Magnesia-Bearing Raw Materials to Obtain Quality Magnesia

机译:一种热机械方法来丰富含镁原料以获得优质镁的可能性

获取原文
获取原文并翻译 | 示例
           

摘要

A thermomechanical method is examined for its potential use in concentrating magnesia-bearing raw materials from the Satka deposit by removing the impure components. It is shown that roasting magnesite within the range 680 - 750A degrees C and its subsequent break-up (abrasion) under certain mechanical loads can increase MgO content in the < 0.5 mm fraction of the roasted product nearly 10%. It is established that dust entrainment is minimal and does not exceed 1.5% when the magnesite is roasted in a fixed bed. This result can be obtained with a tenfold change in the thickness of the bed (from 20 to 200 mm).
机译:通过去除不纯组分,研究了一种热机械方法在从萨特卡矿床浓缩含镁原料中的潜在用途。结果表明,在680-750A摄氏度范围内焙烧菱镁矿及其随后在一定机械负荷下的分解(磨损)会在焙烤产品的<0.5 mm部分中将MgO含量提高近10%。已经证实,当菱镁矿在固定床中焙烧时,粉尘的夹带是最小的并且不超过1.5%。通过将床的厚度改变十倍(从20到200 mm),可以获得该结果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号