首页> 外文期刊>Minerals Engineering >Sample requirements for HPGR testing procedure
【24h】

Sample requirements for HPGR testing procedure

机译:HPGR测试程序的样本要求

获取原文
获取原文并翻译 | 示例

摘要

Green field projects demand relatively large amounts of sample from drill-cores. Besides chemical analysis, samples are required for mineralogy and liberation characterization, physical characterization, concentration tests and a number of tests for crushing and grinding parameters. If the project's process route includes a possible HPGR grinding stage, lab-scale tests for scale-up and variability analysis are required. HPGR grinding characterization can be carried out in a small diameter roll HPGR, such as the LABWAL. Some commercial labs recommend 20-30 kg samples for steady-state tests, but this is a rather large sample from the point of view of a green field project campaign. The question that is being assessed here is how much sample is really required? Surely, the more material that is available the more reliable will be the test results. However, when the sample mass size is reduced, what is the impact on the data that is produced? In this work, six phlogopitite samples weighing 20 kg were tested in the LABWAL HPGR using six initial hydraulic pressures, 10, 20, 30, 40, 50 and 60 BAR. The specific capacity and specific power factors were determined, as well as the critical angle of nip, and the critical gap. Size distributions were measured and size-mass balance parameters were determined for the Austin model under the range of grinding pressures that were produced. With the data, a hypothetical industrial HPGR for the phlogopitite was designed for a standard capacity of 100 t/h and operating at 2 N/mm(2) specific grinding force. The work was then repeated using 10 kg samples and 5 kg samples. Results show that, under the conditions that were chosen, samples weighing 5 kg are sufficient for characterization in the LABWAL HPGR. (C) 2014 Elsevier Ltd. All rights reserved.
机译:绿地项目需要从钻芯获得相对大量的样品。除化学分析外,还需要样品进行矿物学和解放特征,物理特征,浓度测试以及许多破碎和研磨参数测试。如果项目的工艺路线包括可能的HPGR研磨阶段,则需要进行实验室规模的规模放大和变异性分析测试。 HPGR研磨特性可以在小直径的HPGR辊中进行,例如LABWAL。一些商业实验室建议将20-30 kg样品用于稳态测试,但是从绿色领域项目活动的角度来看,这是一个相当大的样品。这里要评估的问题是真正需要多少样本?当然,可用的材料越多,测试结果就越可靠。但是,当减小样本质量大小时,对生成的数据有什么影响?在这项工作中,使用六个初始液压10、20、30、40、50和60 BAR在LABWAL HPGR中测试了六个重20 kg的金云母样品。确定了比容量和比功率因数,以及压区的临界角和临界间隙。在产生的磨削压力范围内,测量了奥斯汀模型的尺寸分布并确定了尺寸-质量平衡参数。利用这些数据,设计了一种用于金云母的假想工业HPGR,其标准容量为100吨/小时,并且在2 N / mm(2)的比磨力下运行。然后使用10千克样品和5千克样品重复该工作。结果表明,在所选条件下,重5 kg的样品足以在LABWAL HPGR中进行表征。 (C)2014 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号