Two series of plasticized PVC formulations were prepared, containing one of the following di (2-ethyl hexyl phthalate)/epoxidized soybean oil ratios (phr/phr): (a) 35/3, (b) 55/3, (c) 45/0 or, (d) 45/6. For each ratio, the following calcium stearate/zinc stearate ratios (phr/phr) were considered: (a) 0.6/0.4, (b) 0.8/0.2 or, (c) 1.0/0.0; all formulations were prepared with a total content of stearate(s) of 1.0 phr. The difference between the series was the preheating of stearates (150 degrees C, 90 min), carried out before the dry-blend preparation. The changes of tensile properties produced by the degradation process were measured in ribbons obtained by extrusion.
机译:制备了两个系列的增塑PVC配方,其中包含以下二邻苯二甲酸二(2-乙基己基邻苯二甲酸酯)/环氧大豆油比率(phr / phr)中的一种:(a)35/3,(b)55/3,(c) 45/0或(d)45/6。对于每个比率,考虑以下硬脂酸钙/硬脂酸锌比率(phr / phr):(a)0.6 / 0.4,(b)0.8 / 0.2,(c)1.0 / 0.0;所有制剂的硬脂酸酯总含量为1.0 phr。系列之间的区别在于硬脂酸酯的预热(150摄氏度,90分钟),是在干混物制备之前进行的。在通过挤出获得的带中测量了由降解过程产生的拉伸性能的变化。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号